Critical Casting Thickness for Formation of Metallic Glass Alloys from Melts - Practical Electron Microscopy and Database - - An Online Book - |
||||||||
Microanalysis | EM Book https://www.globalsino.com/EM/ | ||||||||
This book (Practical Electron Microscopy and Database) is a reference for TEM and SEM students, operators, engineers, technicians, managers, and researchers. | ||||||||
================================================================================= | ||||||||
Figure 3067 shows the critical cooling rate (Rc) and critical casting thickness (dc) for formation of various metallic glass alloys from melts as a function of reduced glass transition temperature (Trg). In general, as the reduced glass transition temperature increases, the required cooling rate for glass formation decreases, and thus it is possible to form thicker glasses at slower cooling rates.
Figure 3067. Critical cooling rate and critical casting thickness for formation of various metallic glass alloys from melts as a function of reduced glass transition temperature.
|
||||||||
================================================================================= | ||||||||
The book author (Yougui Liao) welcomes your comments, suggestions, and corrections, please click here for submission. If you let book author know once you have cited this book, the brief information of your publication will appear on the “Times Cited” page. | ||||||||
|
||||||||